Main station|Member Center|Save the desktop|Mobile browsing
Ordinary Member

Qingyuan Aimen Chemical Co

sell
  • There is no classification
contact
  • Contact:陈俊安
  • Phone:0763-3350486
  • Email:504861133@qq.com
  • fax:0763-6986977
search
 
link
  • There is no link yet
home > sell > Deluxe #188 Series VAC Ink
Deluxe #188 Series VAC Ink
products: Views:4Deluxe #188 Series VAC Ink 
brand: ALPHA
price: 面议
MOQ:
Total supply:
Delivery date: Shipped within 3 days from the date of payment by the buyer
Valid until: Long-term validity
Last updated: 2015-09-09 16:14
 
Details
Luxury
Series
Inks
Luxury series inks are cheap volatile drying inks specially developed for printing on polycarbonate industrial meter plates and nameplate pages. Although this ink is cheap, it is a high-quality ink with high performance and low price.
Promote the printing of polycarbonate acrylic resin materials for automotive letter boards, industrial meter plates, nameplates, etc., as well as the printing of soft and hard wood products.
Characteristics
Won’t crack the material, excellent adhesion
Excellent workability, won’t spread ink and cause pinholes
Good flexibility, can be used for drilling holes, etc. Good post-processing adaptability
Excellent oil resistance, alcohol resistance and chemical resistance.
Physical property table
Test items
Test method
Results
Adhesion
Cross scratch tape peeling test
Passed
Hard< br/>Degree
Pen hardness test
Between
Weather resistance
Resistance to three years of outdoor exposure
No abnormality
Ethanol resistance
/> Used ethanol, friction times back and forth
No abnormality
Grease resistance
Rubbing times with Kao Hand Lotion
No abnormality
Friction resistance
br/> Use a leather-like load, path, and repeated friction
No abnormality in adhesion
Instructions for use: Please use diluent solvent, standard slow drying and extra slow drying. When printing fine line drawings, please use a special slow-drying solvent. Polycarbonate is prone to cracking if other diluting solvents are used.
Use a clean, lint-free cloth covered with luxury film cleaning fluid to wipe the surface of the plastic film. It can effectively remove surface grease and dirt without affecting the plastic film itself.
Dilute the drying solvent and print on it. The finger touch time at room temperature is as follows
Standard solvent is about minutes
Slow drying solvent is about minutes
Extra slow drying solvent is about minutes< br/>Special cracking slow-drying solvent takes about 10 minutes
In order to prevent the residue of bad odor caused by residual solvent when printing on automotive letter plates and industrial meter plates, it is recommended to perform heat drying at ℃ or above.
Please use luxury cleaning solvent to clean and wipe the screen.
Color packaging There are more than 6 colors to choose from, each canned.
Cautions Polycarbonate molded products and some sheets are prone to cracking. If cracking occurs, please anneal the material to improve it. If cracking occurs, use our company's special solvent to improve it.
The technical parameters of this information were measured under the conditions of our company. However, since the conditions and methods of using our products are beyond our control, we cannot guarantee or guarantee the technical parameters and suggestions provided. The company is not responsible for possible losses and damages. Users are requested to conduct necessary tests before use.